Recommendations on Scales

Post by Shell Kurtis »

I'm looking to buy a scale to use accurately measure glue mixtures, glass for casting and metal for casting. Any recommendations on scales?

Thanks in advance :D

Shell
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Buy a postal scale. They're accurate and widely available.
Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Re: Recommendations on Scales

Post by Paul Tarlow »

Shell wrote:I'm looking to buy a scale to use accurately measure glue mixtures, glass for casting and metal for casting. Any recommendations on scales?

Thanks in advance :D

Shell

http://www.oldwillknott.com/
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Post by rosanna gusler »

if you know anyone in weightwatchers tm get one of their scales. weighs in gm or lb and has tare function,accurate to .2gm about 20$ rosanna
Shell Kurtis
Posts: 7
Joined: Thu Mar 13, 2003 8:47 pm
Location: Ellicott City, Maryland

Recommendations on Scales

Post by Shell Kurtis »

Thanks for the recommendations. One last question. I was made to believe that in order to mix Hxtal properly you needed a REALLY Accurate scale, preferably digital. Is this correct? Can I really get by on a postal scale?

Thanks again,
Shell
Jerry Barnett
Posts: 55
Joined: Wed Mar 12, 2003 11:40 am
Location: Texas, USA

Post by Jerry Barnett »

I use an Ohaus triple beam balance scale for mixing Hxtyl. It is not digital. It measures in grams.

The accuracy of the scale becomes important when you are:

1) Mixing small quantities

2) Correcting the first mix when you overshoot in adding the second part.

Jerry