What kind of tools I need?
In my kiln cast sculptures I have large surfaces
that are slightly curved - convex nac concave.
What are the proper tools for grinding and polishing?
Just now I have nothing but two grades of diamond pad,
1000 grit wet'n'dry paper and a piece of chamoise
to use with aluminium oxide.
The hand polishing keeps me unhealthy long
times in front of telly. Suggestions for inexpensive
power tool solution?
-lauri
Q: polishing curved surfaces?
Moderators: Brad Walker, Tony Smith
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Q: polishing curved surfaces?
Have a look over Hislauri wrote:What kind of tools I need?
In my kiln cast sculptures I have large surfaces
that are slightly curved - convex nac concave.
What are the proper tools for grinding and polishing?
Just now I have nothing but two grades of diamond pad,
1000 grit wet'n'dry paper and a piece of chamoise
to use with aluminium oxide.
The hand polishing keeps me unhealthy long
times in front of telly. Suggestions for inexpensive
power tool solution?
-lauri
http://www.hisglassworks.com/index.html
Much of the time I use a battery powered drill with pads attached

-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Grinding and polishing
Thanks Brian, I had forgottn that.
It does not work in winter, when the roads are icy.
I have a Dremel, but have to find diamond pads for it.
-lauri
It does not work in winter, when the roads are icy.
I have a Dremel, but have to find diamond pads for it.
-lauri
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Grinding and polishing
Works better in winter the water keeps it coollauri wrote:Thanks Brian, I had forgottn that.
It does not work in winter, when the roads are icy.
I have a Dremel, but have to find diamond pads for it.
-lauri
But better the ice is an added coolant n U can go faster
If U cant buy what U want U can buy the diomond pads n stick em on n make ur own