Anyway, the cracks are in the exact same spots on both side. They effectively cut off the sides of the round circle making it sort of like a rectangle with round edges on the shorter sidse. I am pretty sure that it is from the extra holes we drilled. I may have put too many. We probably added aboout 6-8 holes (can't remember exactly and I can't look), but I took them around around the one hole provided, 2 there I think and then made a square of holes around those, all about 2-3 inches above the other, heading up to the sides and to edges of the mold. I am thinking that there are holes (1 on each side possibly) right along the horizontal line that the glass cracked in
![Brick wall ](*,)](./images/smilies/eusa_wall.gif)
My schedule was beyond conservative so I don't think it was that. 50 dph set 1130 hold 30 minutes, and this was the fourth firing at this rate. This piece has been in my kiln since Saturday!!!
So please learn from me, do not put your holes within the last 2-3 inches of a mold, near the edges and top sides of the mold.
Aimee
aka
Anea
![Sad :(](./images/smilies/icon_sad.gif)