EMBOSSING,,,,,,,,,,,,,,,,,,,,,,what is the tool

Post by rodney »

can anyone tell me about the embossing, what is the tool made of, is it like a graphite masher, would a simple plaster cast work,
thanks,,,rodney
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

The commercial embossing products are brass. Plaster won't withstand repeated use at the necessary temperature (1300 to 1400 F).
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: EMBOSSING,,,,,,,,,,,,,,,,,,,,,,what is the tool

Post by Bert Weiss »

rodney wrote:can anyone tell me about the embossing, what is the tool made of, is it like a graphite masher, would a simple plaster cast work,
thanks,,,rodney
Rodney

What I call embossing is also referred to as kiln carving. I use Unifrax 970 paper that is 1/32" thick. You cut the paper and layer it up, then fire over it. Any pattern that you can cut with a razor knife can be embossed on the glass.

Bert