I have the large used Jen-Ken "bathtub" oval, and recently bought a Paragon UDC 2000 controller, a real work horse, used. We installed it and tried it out. The controller temperature and the kiln temperature readings were very different, and got more different the higher the temperature went, until the controller said 2400 degrees and turned itself off, and the kiln said 450. I talked with the guy who sold me the controller and he said there might be a problem with the setting for the thermocouple. We checked that, that wasn't it. Then we replaced the thermocouple.
I tried it again tonight, and it's not as bad, but the controller temperature is still about 100 degrees higher than the reading on the kiln.
Do you have any idea what's happening? Or what we can do?
Any help you could give would be appreciated.
Thanks.
kiln controller problems
Moderators: Brad Walker, Tony Smith
-
jen prentiss
- Posts: 3
- Joined: Fri Jun 06, 2003 12:30 am
- Location: Los Angeles, CA
- Contact:
-
Phil Hoppes
- Posts: 298
- Joined: Wed Mar 12, 2003 2:20 pm
- Location: Overgaard, AZ
What type of thermocouple did you buy? I'm guessing that the Paragon wants a type K thermocouple. If you did not buy a type K but instead got a type J or something else, the thermocouple and controller will act like they are working together but you will get incorrect temperature readings. This sounds like the problem you are having.
Phil
Phil
-
jen prentiss
- Posts: 3
- Joined: Fri Jun 06, 2003 12:30 am
- Location: Los Angeles, CA
- Contact:
-
Phil Hoppes
- Posts: 298
- Joined: Wed Mar 12, 2003 2:20 pm
- Location: Overgaard, AZ
You can't tell by looking, either on the thermocouple or the controller. For the controller, I'm assuming you got some manuals or documentation with them. I would look through the doc's and at least confirm the thermocouple type required by the controller. Then I would call the place you got your thermocouple from and ask them what they sold you. They should be able to tell you as there is a difference. Not all thermocouple are the same. If you don't get any satisfaction from your thermocouple supplier I would check out Omega at the following link.
http://www.omega.com/ppt/pptsc.asp?ref=ICIN&Nav=tema04
If you need some help in selecting the type of thermocouple you might need send me an email and I'll help you out.
Phil
http://www.omega.com/ppt/pptsc.asp?ref=ICIN&Nav=tema04
If you need some help in selecting the type of thermocouple you might need send me an email and I'll help you out.
Phil