Taking into account the glass AREA when annealing...
Moderators: Brad Walker, Tony Smith
-
Catharine Newell
- Posts: 83
- Joined: Thu Mar 13, 2003 12:33 am
- Location: Portland, OR
Taking into account the glass AREA when annealing...
Without resorting to a complex mathematical formula, how do I compute an anneal soak for AREA + thickness of a panel? For example: 35x14x5/8"... It has come to my attention that I am not paying enough attention to the area of glass involved when programming my soak at 960. BE glass, top and side elements, fibre shelf, 46dph from 960-775, 70dph to 500...
What d'you say?
Catharine
What d'you say?
Catharine
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Taking into account the glass AREA when annealing...
CatherineCatharine Newell wrote:Without resorting to a complex mathematical formula, how do I compute an anneal soak for AREA + thickness of a panel? For example: 35x14x5/8"... It has come to my attention that I am not paying enough attention to the area of glass involved when programming my soak at 960. BE glass, top and side elements, fibre shelf, 46dph from 960-775, 70dph to 500...
What d'you say?
Catharine
In my float glass work, I ignore area and anneal for thickness. When I put the largest piece of 10mm glass that will fit in my kiln in to the tempering furnace and it heated to 1100ºF in 5 minutes without breaking, I figure that my schedules are working.
I think that the part of the schedule that you need to worry most about is heatup. The various stresses caused by different glasses pushing and pulling on one another is going to be more problematic relative to heatshock than it will have a problem equalizing in temperature when annealing.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
As I understand, the *area* is relevant only to a side
element kiln. The heath escapes the shortest way. A flat
sheet loses heat over the top surface, and maybe thru the
shelf. I do believe that even the shelf is cooled mainly
thry the glass.
*Under* a large sheet near the bottom of the kiln, there
may be a hot air pocket, releasing heath only around
sides, that may cause uneven annealing and warrant
a slower pace.
I need both elements to reach the fusing
temperature, but I use only the top element for annealing.
This prevents the top surface cooling too fast, and helps
to keep the temp even thru the thickness of glass+mold+shelf.
-lauri
element kiln. The heath escapes the shortest way. A flat
sheet loses heat over the top surface, and maybe thru the
shelf. I do believe that even the shelf is cooled mainly
thry the glass.
*Under* a large sheet near the bottom of the kiln, there
may be a hot air pocket, releasing heath only around
sides, that may cause uneven annealing and warrant
a slower pace.
I need both elements to reach the fusing
temperature, but I use only the top element for annealing.
This prevents the top surface cooling too fast, and helps
to keep the temp even thru the thickness of glass+mold+shelf.
-lauri
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Taking into account the glass AREA when annealing...
In additionCatharine Newell wrote:Without resorting to a complex mathematical formula, how do I compute an anneal soak for AREA + thickness of a panel? For example: 35x14x5/8"... It has come to my attention that I am not paying enough attention to the area of glass involved when programming my soak at 960. BE glass, top and side elements, fibre shelf, 46dph from 960-775, 70dph to 500...
What d'you say?
Catharine
Go 4 the thickest area
It thick / thin go 4 the thickest area then add a bit

-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Taking into account the glass AREA when annealing...
Thick and thin is a totally different problem than uniform thickness. Stress is relieved when the entire piece of glass stabilizes at the right temp. Thick and thin takes longer to do that than just thick.Brian and Jenny Blanthorn wrote:In addition
Go 4 the thickest area
It thick / thin go 4 the thickest area then add a bit
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Catharine Newell
- Posts: 83
- Joined: Thu Mar 13, 2003 12:33 am
- Location: Portland, OR
Well then, if top and side elements are in use during the entire firing, am I correct in understanding that my main concern is the thickness of a relatively uniform panel rather than area? I'm thinking that area must have something to do with this process. Re: the 35x14x5/8 panel I mentioned... I'm soaking for 2:30 @960, then doing the drop I mentioned in the first post. Does this sound appropriate, or too short at 960? I generally take 8:30 plus to reach my tack/full fuse temps...
Catharine
Catharine
-
Catharine Newell
- Posts: 83
- Joined: Thu Mar 13, 2003 12:33 am
- Location: Portland, OR
Let me amend this to say that I take 9:30, at least, to reach targeted temps[/u]Catharine Newell wrote:Well then, if top and side elements are in use during the entire firing, am I correct in understanding that my main concern is the thickness of a relatively uniform panel rather than area? I'm thinking that area must have something to do with this process. Re: the 35x14x5/8 panel I mentioned... I'm soaking for 2:30 @960, then doing the drop I mentioned in the first post. Does this sound appropriate, or too short at 960? I generally take 8:30 plus to reach my tack/full fuse temps...
Catharine
I always try to think like the glass and like the kiln. A piece of glass wants to be the same temp throughout. Going up and down the kiln must accomplish that. If a kiln has only top elements and fibre board is under the piece than cooling could go faster. When you put side elements on, the edges are getting more heat than the center even if top elements are on as well. A kiln shelf retains heat much longer than fibre board, therefore when a kiln shelf is used, the bottom of the piece will be significantly hotter than the top of the piece. For me the ideal situation is fibre board below and only top elements. If the kiln has side elements I baffle all around. All this being said, after putting 3 or 4 weeks into a piece, I never hesitate to err on the side of caution..................steve
Steve Klein Studio
1650 N. Glassell, Studio U
Orange, CA 92867
1650 N. Glassell, Studio U
Orange, CA 92867
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
SteveS. Klein wrote:I always try to think like the glass and like the kiln. A piece of glass wants to be the same temp throughout. Going up and down the kiln must accomplish that. If a kiln has only top elements and fibre board is under the piece than cooling could go faster. When you put side elements on, the edges are getting more heat than the center even if top elements are on as well. A kiln shelf retains heat much longer than fibre board, therefore when a kiln shelf is used, the bottom of the piece will be significantly hotter than the top of the piece. For me the ideal situation is fibre board below and only top elements. If the kiln has side elements I baffle all around. All this being said, after putting 3 or 4 weeks into a piece, I never hesitate to err on the side of caution..................steve
I couldn't agree more on every point.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
CORRECTION
Just learned it by the hard way!
The area does count ! !
Take a one inch button and a ten inch plate.
What ever is the residue of stress after annealing,
in the 10" plate it has a tenfold moment to break
the glass. So you must be more careful in annealing.
This applies to the warm up stage, too.
As Lani stated earlier, it is possible to "over anneal" in
a kiln with uneven temp distribution. You are just keeping
on the difference.
In a kiln with nearly perfect evenness, the cooling
takes place all over the piece simultaneously.
-lauri
The area does count ! !
Take a one inch button and a ten inch plate.
What ever is the residue of stress after annealing,
in the 10" plate it has a tenfold moment to break
the glass. So you must be more careful in annealing.
This applies to the warm up stage, too.
As Lani stated earlier, it is possible to "over anneal" in
a kiln with uneven temp distribution. You are just keeping
on the difference.
In a kiln with nearly perfect evenness, the cooling
takes place all over the piece simultaneously.
-lauri