Good evening,
I am looking for a large grinder polisher (18 inch diameter).
Is anyone familiar with or has anyone done business with SW Diamond Products in Gorman, California? I was given one of their brochures but haven't found anyone who has done business with them before.
Your comments or suggestions would be appreciated.
Zoe
Grinder/Polishers
Moderators: Brad Walker, Tony Smith
Grinder/Polishers
Thanks, Marty,
I will check into that.
Zoe
I will check into that.
Zoe
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
SW has a great grinder. Has the advantage of the water feed coming through the center of the wheel which means you get an even wetting of the grinding disc and with their design, you can use the entire surface of the disk right through the center since they have no post or anything else in the way. Particularly useful if you are working on large pieces. You might consider the fact of not needing to buy as big a machine from them as buying one elsewhere. A 12 inch wheel will let you grind the full width of the wheel evenly wet as compared to perhaps only 5 and a half on a center post model. The smaller magnetic diamond pad wheels cost less than the bigger machine ones. Ask if they have any lubricating system developed for the shaft. Could someone post/private email me their address/contact information as I lost that and my SW machine in a divorce.
Be sure if you buy one, to remove the magnetic diamond disc and to dry the wheel etc. each time after use or you will get rust!
Be sure if you buy one, to remove the magnetic diamond disc and to dry the wheel etc. each time after use or you will get rust!
-
Kathie Karancz
- Posts: 137
- Joined: Wed Mar 12, 2003 3:49 pm
- Location: Calgary, Alberta, Canada
- Contact:
Hey guys: funny that your talking about this....
I have an opportunity to buy the following for $600.00 Canadian - should I - don't have a clue about glass polishers.
Thanks for any feedback
Kathie
I have the following cold working equipment for sale
Listed is the retail price on these items
Beaver arbour-----------------------------------------300.00
Two expandable rubber belt holders--------------206.00
1x8 inch diamond-grinding wheel-----------------300.00
1x8 inch aluminums oxide wheel-------------------230.00
aprox forty different grain belts -----------------160.00
3 polishing felt wheels------------------------------125.00
¾ horse motor for arbour------------------------------75.00
New price 1396.00
Selling for 700.00
[/u][/b]
I have an opportunity to buy the following for $600.00 Canadian - should I - don't have a clue about glass polishers.
Thanks for any feedback
Kathie
I have the following cold working equipment for sale
Listed is the retail price on these items
Beaver arbour-----------------------------------------300.00
Two expandable rubber belt holders--------------206.00
1x8 inch diamond-grinding wheel-----------------300.00
1x8 inch aluminums oxide wheel-------------------230.00
aprox forty different grain belts -----------------160.00
3 polishing felt wheels------------------------------125.00
¾ horse motor for arbour------------------------------75.00
New price 1396.00
Selling for 700.00
[/u][/b]