I have a Skutt 1018 side firing ceramic kiln that I am using for glass. My Skutt book says to always leave the top peep hole unplugged. I read in one of the posts to plug all holes to avoid drafts, so my question is can I plug all the holes and not hurt my kiln? Does the leaving one unplugged only apply when firing clay?
Thanks,
Sharon
Closing Peep holes
Moderators: Brad Walker, Tony Smith
-
Sharon Lee
- Posts: 13
- Joined: Thu May 08, 2003 11:05 am
- Location: Roseville, CA
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Closing Peep holes
If a none thermal shock problem fire I keep all bungs out till about 700 / 750 CSharon Lee wrote:I have a Skutt 1018 side firing ceramic kiln that I am using for glass. My Skutt book says to always leave the top peep hole unplugged. I read in one of the posts to plug all holes to avoid drafts, so my question is can I plug all the holes and not hurt my kiln? Does the leaving one unplugged only apply when firing clay?
Thanks,
Sharon
Then put em in

-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Closing Peep holes
I can't imagine that it would hurt the kiln to plug the holes. Do what is best for your glass. If you are firing enamel or glue or plaster, along woth your glass, leaving a hole for gasses to escape is good.Sharon Lee wrote:I have a Skutt 1018 side firing ceramic kiln that I am using for glass. My Skutt book says to always leave the top peep hole unplugged. I read in one of the posts to plug all holes to avoid drafts, so my question is can I plug all the holes and not hurt my kiln? Does the leaving one unplugged only apply when firing clay?
Thanks,
Sharon
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions