Re: Surface questions

Post by Kev »

I've fired on thinfire then flipped and firepolished it. I then sandblasted the surface and did a light brief fire polish on it and achieved a very low gloss satin finish.
Attachments
DSC01221.JPG
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Surface questions

Post by Marty »

Not fair! I saw the post and thought Jackie had come back.....
Then I saw the date.
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Surface questions

Post by The Hobbyist »

Yup, the excitement was dispelled all too soon.

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Surface questions

Post by DonMcClennen »

What is the point of this post on a 9 yr old thread????????? Hopefully we've moved on as Jackie did!