Re: MESH MELT DISASTER
Posted: Sun Sep 23, 2012 3:07 am
Havi, you're correct. The mesh is twist-tied to the rebar and the rebar just sits on the mullite cross pieces.
Jim
Jim
Guide to fusing, slumping, and related kilnforming techniques
https://warmglass.com/phpBB3/
Dairy,Dairy Queen wrote:Havi, I roll out a 1 inch thick slab of clay. I cut out and remove circles or slots, at least 1 inch wide. After the clay dries, I fire it to cone 6. Normally, I don't fire clay molds, but I am asking this piece to support the weight of the stacked glass, and I don't want any of the clay material to drop with the glass. Impossible to remove.