making cabochon with coin inclusion?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Tom Fuhrman
Posts: 187
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: making cabochon with coin inclusion?

Post by Tom Fuhrman »

I used to put copper pennies in bottles and paperweights when I had my furnace. I would make a small indentation/cup in the gather then insert the coin and attach a 2nd gather on the cup's edge to encapsulate the coin. For fusers I would try making a small cup shape and then put the copper penny in and tack fuse a flat disc on the cup. Copper pennies are those that are classified as
wheat" pennies. I just found a jar with several hundred in a box I had stored and forgot I had.
Putting a coin in a small bottle shape on a torch should be quite easy. Seal off a tube, insert coin , seal other end tubing. Solid copper coins seem to work best just as inclusions of copper wire are easy to do.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: making cabochon with coin inclusion?

Post by Brad Walker »

Don't try this with pennies made after 1983 -- they're zinc, not copper. Pennies made before 1983 are copper, and pennies made in 1983 could be either.