I find it really interesting how some people here get totally worked up about a small amount of glass dust, while in industry there is a crazy amount of glass dust in glass factories EVERYWHERE. An awful lot of these shops are scrutinized heavily by OSHA and other government boards yet no one has a problem with it. Try going into a granite counter top manufacturer there is a good chance you can't see the far side of the shop through the haze (slight exaggeration)
(FACT) glass dust DOES NOT give you silicosis, There is a huge difference between amorphous silica and crystaline silica. Crystaline is harmful and amorphous is considered a nuisance. The silica in glass is crystaline until it's been melted into a glass, that process makes it amorphous. That doesn't mean it's good to breath huge amounts of it in however. You are literally breathing deadly gases and fumes right now, you are not dropping like flies.
It's the dose that makes the poison.
Fun fact the most paranoid person I know regarding glass dust smokes 2 packs a day and drinks like a fish. Go figure