Does anyone have a firing schedule for hanovia mother of pearl luster? Last night I tried it out - I took it up to 1310, held for ten minutes. Unfortunately, what I ended up with is an etched look - definately not mother of pearl. I think I probably took it too high and it burned off. Anyone else ever use the stuff? Thx.
Posted: Sat May 31, 2003 3:04 pm
by Cynthia
http://clayartcenter.com/glaze_hanova.htm
I think it's cone 018-019. Call your ceramics folks for a conversion if you need one since I don't know what temp that is. Info about all hanovia products and firing cones are at the above link.
Posted: Sat May 31, 2003 3:22 pm
by Rob Morey
cone 018 to 019 would average out to be right about 1250 F.
Here's a useful chart to explain cone temp.
http://www.bigceramicstore.com/Informat ... Chart.html
Rob
Posted: Sat May 31, 2003 11:31 pm
by Barbara Muth
I apply the lusters when I slump.
barbara