Page 1 of 1
					
				Uroboros Glass Frit Mosaic
				Posted: Wed Jun 11, 2003 6:02 pm
				by Betty
				Just got Uroboros glass frit Mosaic size, and it has a white powder or dust all over the glass pieces.  Do I need to remove the dust from the pieces?
The glass i fired last night I cleaned with rubbing alocolce and it looked good this morning.
Betty
			 
			
					
				
				Posted: Thu Jun 12, 2003 12:35 am
				by Cynthia
				I'd wash it.  I would think it's glass or silica dust from the crushing process that is all over your frit, but you can't be certain.  Just to get the silica dust out would be motive enough, but you don't know how it will fire up if you don't clean it either.  I would put it in a cheese cloth and rinse it off well then dry with a clean cotton cloth.
For the smaller frit it has never created problems for me, but for the larger chunks, I am guessing it might make a visible difference.
			 
			
					
				
				Posted: Thu Jun 12, 2003 12:53 am
				by Lynne Chappell
				Yes, I think Cynthia is right. The really fine dust can cause clouding.
			 
			
					
				
				Posted: Thu Jun 12, 2003 9:26 am
				by Betty
				Thank You, better to ask and better to not take the chance
Thanks 
Betty
			 
			
					
				ASK Uro!
				Posted: Thu Jun 12, 2003 6:36 pm
				by Cheryl
				I would call Uro directly and ask them if this is what you can expect all the time - because that's a big pain!! Maybe you got a bum batch.