Page 1 of 1
					
				melt pot
				Posted: Tue Jun 17, 2003 3:23 pm
				by Betty
				I want to try the melt pot,
 Do i need kiln wash on the melt pot (aka flower pot)?  all these scarpes it is nice to use them up.
			 
			
					
				
				Posted: Tue Jun 17, 2003 6:43 pm
				by Rob Morey
				No, do not kiln wash the pot or the kiln wash will flow into the glass and ruin it. You do need to have a good layer of kiln wash on your shelf and I also kiln wash any furniture that I use to hold up the pot, just in case. Once the pot is cool, lift it out by lifting the glass off the kiln shelf and score the “dripâ€
			 
			
					
				
				Posted: Wed Jun 18, 2003 9:30 pm
				by Betty
				Thank you, as soon as I get the supports to hold the pot i will do this.