HELP: Clear Float Fusing
Moderators: Brad Walker, Tony Smith
-
phlava
HELP: Clear Float Fusing
Does anyone have a profile for fusing 2 layers of 3/4" thick clear float glass together (total of 1-1/2" thickness)? The glass size is 3' x 7'. I appreciate any input you may have.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Phlava
I am uncomfortable giving out such important information to an anonymous poster with no contact info available. Edit your bio with Brad and I'll answer your question.
This may sound nasty but this community is one of trust and sharing and if you don't identify yourself or enable Email, in my opinion, you are the one not to trust.
I realize that somebody new here might not be aware of an issue like this, and for that I apologize. I think that bringing this up will help clue people in.
Bert
I am uncomfortable giving out such important information to an anonymous poster with no contact info available. Edit your bio with Brad and I'll answer your question.
This may sound nasty but this community is one of trust and sharing and if you don't identify yourself or enable Email, in my opinion, you are the one not to trust.
I realize that somebody new here might not be aware of an issue like this, and for that I apologize. I think that bringing this up will help clue people in.
Bert
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
FYI
I did communicate with Phlava off line. If anybody is dieing to know the answer to her question, I can post it.
I did communicate with Phlava off line. If anybody is dieing to know the answer to her question, I can post it.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions