Does anyone know what BE recommends for 3/4" thick?
I have Graham's schedule -- just wondering how it compares to BE's recommendation.
- Paul
Thick BE annealing question
Moderators: Brad Walker, Tony Smith
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
Lani has all the good stuff online these days
http://www.bullseyeconnection.com/pdfs/ ... _thick.pdf
More here, the Tech Notes are online too, bottom of the page.
http://www.bullseyeconnection.com/getsmart.html
Ron
http://www.bullseyeconnection.com/pdfs/ ... _thick.pdf
More here, the Tech Notes are online too, bottom of the page.
http://www.bullseyeconnection.com/getsmart.html
Ron