can anyone tell me about the embossing, what is the tool made of, is it like a graphite masher, would a simple plaster cast work,
thanks,,,rodney
Glass embossing
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1540
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: EMBOSSING,,,,,,,,,,,,,,,,,,,,,,what is the tool
Rodneyrodney wrote:can anyone tell me about the embossing, what is the tool made of, is it like a graphite masher, would a simple plaster cast work,
thanks,,,rodney
What I call embossing is also referred to as kiln carving. I use Unifrax 970 paper that is 1/32" thick. You cut the paper and layer it up, then fire over it. Any pattern that you can cut with a razor knife can be embossed on the glass.