18" x 9" x 1"
If I soak it at 1000F (to ensure the entire piece is safely above the strain point and won't thermal shock) and then go up real fast to fire polish do I need to dam the piece?
The whole thick thing is new for me.
- Paul
Fire Polishing Thick
Moderators: Brad Walker, Tony Smith
-
Paul Tarlow
- Posts: 344
- Joined: Sun Mar 09, 2003 4:06 pm
- Location: Helios Kiln Glass Studio - Austin
- Contact:
Re: Fire Polishing Thick
i've not worked with anything thicker than 1/2" thick slabs at times but if you are only going high enuf to fp edges or even start them rounding - in my 24" jen ken this is between 1250 deg and 1300 deg depending on look - i don't dam the piece - sometimes lower and longer is the best course when in doubt - if it's under fp'd you can always put it back in.....Paul Tarlow wrote:18" x 9" x 1"
If I soak it at 1000F (to ensure the entire piece is safely above the strain point and won't thermal shock) and then go up real fast to fire polish do I need to dam the piece?
The whole thick thing is new for me.
- Paul
D
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Fire Polishing Thick
I would use a combination of these technologiesPaul Tarlow wrote:18" x 9" x 1"
If I soak it at 1000F (to ensure the entire piece is safely above the strain point and won't thermal shock) and then go up real fast to fire polish do I need to dam the piece?
The whole thick thing is new for me.
- Paul
Assuming U got side elements
Baffle n Go tm To keep the body of the glass cool
Zap n Blastem To fire polish the surface
I suggest a 220 grit finish then 280 sandblast or better
Unless U over fire the glass will not pool