Page 2 of 2
Re: Surface questions
Posted: Thu Jul 12, 2012 9:01 pm
by Kev
I've fired on thinfire then flipped and firepolished it. I then sandblasted the surface and did a light brief fire polish on it and achieved a very low gloss satin finish.
Re: Surface questions
Posted: Fri Jul 13, 2012 8:53 pm
by Marty
Not fair! I saw the post and thought Jackie had come back.....
Then I saw the date.
Re: Surface questions
Posted: Fri Jul 13, 2012 9:59 pm
by The Hobbyist
Yup, the excitement was dispelled all too soon.
Jim
Re: Surface questions
Posted: Sat Jul 14, 2012 12:31 pm
by DonMcClennen
What is the point of this post on a 9 yr old thread????????? Hopefully we've moved on as Jackie did!