Post by Paul Housberg »

Wondering who out there is doing architectural and site-specific kilnformed glass (as opposed to work which is meant for a gallery). I know you are, Bert, and BJ Katz, - there must be others.

Post a reply or send an email. Thanks.
Image
Paul Housberg
Glass Project, Inc.
Art Glass Feature Walls
http://www.glassproject.com
http://www.facebook.com/housberg
Kitty
Posts: 444
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Post by Kitty »

bullseye gallery now showing related works: http://www.bullseyeconnectiongallery.com/

also, bullseye mentions this:
http://www.pilchuck.com/educational_pro ... (1.5).html

also you might like looking at non-fused architectural glass panels made in dalle de verre method. google it ... i don't have any specific links to share with you, unfortunately.
charlie holden
Posts: 260
Joined: Thu Mar 13, 2003 8:26 pm
Location: Atlanta

Post by charlie holden »

This week I'll complete a baptismal font (a big bowl) that was designed by an architect for a specific site in a church. And I do a lot of light fixtures. I don't think that really qualifies me as the type of specialist you're asking about though.

I took Warren Langley's class at Pilchuck earlier this summer so I'm thinking about going into truly large scale work. But that might require that I take on a partner/investor so I can build another, bigger kiln and take advantage of someone that knows something about business and selling. I'm a good problem solver, not a good organizer.
Paul Housberg
Posts: 103
Joined: Fri Mar 21, 2003 1:08 pm
Location: Rhode Island
Contact:

Post by Paul Housberg »

Kitty wrote:bullseye gallery now showing related works: http://www.bullseyeconnectiongallery.com/

also, bullseye mentions this:
http://www.pilchuck.com/educational_pro ... (1.5).html

also you might like looking at non-fused architectural glass panels made in dalle de verre method. google it ... i don't have any specific links to share with you, unfortunately.

Specifically wondering who on this board is doing architectural stuff - and, specifically involving or incorporating kilnformed glass.
Image
Paul Housberg
Glass Project, Inc.
Art Glass Feature Walls
http://www.glassproject.com
http://www.facebook.com/housberg
Carol
Posts: 112
Joined: Sun Mar 09, 2003 5:48 pm
Location: Thetis Island, BC, Canada
Contact:

Post by Carol »

[quote="Paul Housberg
Specifically wondering who on this board is doing architectural stuff - and, specifically involving or incorporating kilnformed glass.[/quote]

Hi Paul

I've been doing kilnformed accents for my stained glass commissions and carved panels, am currently working on my commission for fused panels in a custom door and am heading for architectural work...I will be having a large kiln built in January for that purpose.

I love mixing the techniques together.

Carol (Swann)
Annah James
Posts: 44
Joined: Wed Jun 25, 2003 12:11 am
Location: Eugene, OR
Contact:

Post by Annah James »

I have been doing architectural glass for a couple of years now - tile murals, cabinet doors, windows, large panels for commercial spaces...I'd really like to get into some lighting!
Currently I am working on an installation for the U of O - a lot of tiles glued to plate glass panels and backlit. I keep working larger and larger. That bigger kiln is getting closer, too!
Are you doing architectural work yet, yourself?
-Annah
Annah James
Posts: 44
Joined: Wed Jun 25, 2003 12:11 am
Location: Eugene, OR
Contact:

Post by Annah James »

So of course, I wrote my reply and hadn't yet looked at your website. Duh!

Neat work!
-Annah
John

Post by John »

That is the market I am aiming for!!!! :D
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Post by Don Burt »

Carol wrote: clip
I've been doing kilnformed accents for my stained glass commissions
clip
I love mixing the techniques together.

Carol (Swann)
Me too

Don Burt
Harry
Posts: 13
Joined: Fri Mar 14, 2003 2:19 am
Location: Portland OR

Post by Harry »

We have been adding larger kilns and doing more architectural commissions. With our waterjet we cut many of the large pieces for the present Bullseye show. Harry Waterjet Design Hillsboro, OR.