I've been experimenting with dichro in making bracelets. I just received a full sheet of DT2 pattern on Bullseye Thin Black glass from CBS. Now for the dumb question:

When fired, will the obvious pattern diffuse? ie: will the dots blend out?

Posted: Sun Jul 27, 2003 12:27 am
by Kitty
i dont think so ... i had a piece of this as a sample, the bigger dots, and they stayed crisp.

Posted: Sun Jul 27, 2003 12:30 am
by Lorelei
ugh... I was soooo hoping. (not real thrilled with dots) I guess I could always rake it about with a BBQ fork eh?

Posted: Sun Jul 27, 2003 12:52 am
by Kitty
someone else once mentioned that they had designed a pendant featuring a single dichroic dot. that could look good, especially if you put a piece of clear over the dot to add depth.

if the dots were on clear instead of black, you could overlay them upside down on other dichro, and probably get a neat effect. i dont use dichro on black, so i'm not much help in offering tips.

Posted: Sun Jul 27, 2003 5:27 am
by Tony Smith
Lorelei,

Did you buy directly from CBS? You might call them and ask them if you can return it for a solid or one of their other patterns... as long as the sheet is undamaged, uncut, etc... they may take it back... you never know unless you ask.

Tony

Posted: Sun Jul 27, 2003 10:57 am
by Lorelei
Unfortunately I didn't buy this direct. I'll contact the place I did and see if they'll exchange it. Thanks for the info everyone.