I have two studios with a Bevel Max machine in one and a Convertible Max machine at the other. They have different size center openings. I don't like the grinding discs that come with the machines. Instead of a disc with diamond grit over the entire surface, they have circles of grinding material on the disc. I need a source for new discs. Linda

Re: grinding discs

Posted: Wed Mar 19, 2003 5:18 am
by Brian and Jenny Blanthorn
Linda Hassur wrote:I have two studios with a Bevel Max machine in one and a Convertible Max machine at the other. They have different size center openings. I don't like the grinding discs that come with the machines. Instead of a disc with diamond grit over the entire surface, they have circles of grinding material on the disc. I need a source for new discs. Linda
Try

http://www.hisglassworks.com/index.html