Saw blade
Posted: Wed Aug 27, 2003 9:01 pm
by Jack Bowman
I'm ready for a new 10" tile saw blade. I have checked the archives but couldn't find reports on MK lapidary blades. Anybody using this grade of blade or know anything about it. Main use would be pattern bar cutting. Daily.
Thank you,
Jack
Re: Saw blade
Posted: Wed Aug 27, 2003 11:02 pm
by dee
Jack Bowman wrote:I'm ready for a new 10" tile saw blade. I have checked the archives but couldn't find reports on MK lapidary blades. Anybody using this grade of blade or know anything about it. Main use would be pattern bar cutting. Daily.
Thank you,
Jack
jack, have a 7" blade mk saw and use their 215gl glass blade regularly to cut slabs and love the blade - i keep it refreshed with a silicon carbide block that i get at lowes - have the 303 professional blade but i think i got the wrong arbor size and haven't had a chance to call mk customer service yet so haven't installed that one...
D
Re: Saw blade
Posted: Thu Aug 28, 2003 5:54 am
by Brian and Jenny Blanthorn
Jack Bowman wrote:I'm ready for a new 10" tile saw blade. I have checked the archives but couldn't find reports on MK lapidary blades. Anybody using this grade of blade or know anything about it. Main use would be pattern bar cutting. Daily.
Thank you,
Jack
I like the MK 297 notched blade but this is for big stuff
4 small rods U might prefer a smooth rimmed one
http://www.mkdiamond.com/lapidary/00_fs.html
U could ask His
http://www.hisglassworks.com/pages/bladeindex.html
Brian