				can anyone tell me where I can buy pyro bars 016--017---018  so I can use my larger kiln for fusing and slumping 

 
			 
			
					
				Re: pyro bars
				Posted: Wed Mar 19, 2003 11:24 pm
				by Ron Coleman
				tattooedpanda wrote:can anyone tell me where I can buy pyro bars 016--017---018  so I can use my larger kiln for fusing and slumping 

 
Here's a link to a source of ceramic cones.
http://www.clayartcenter.com/kilnaccess_cones.htm
The cones are not the best way to fire glass because they will not allow you to soak at fusing temperature.
A better investment is a pyrometer and thermocouple as seen in the attached link below.
http://www.cdvkiln.com/menucctherm.htm
 
To operate your kiln you will still need to install a pyro cone to get the kiln to run.  Select one that will not shut the kiln off at fusing temperatures.  It will be your job to tend the kiln and determine when your glass is fired.
You can also buy a plug-in digital controller at the following link.
http://www.cdvkiln.com/menuccremo.htm