I have been hunting around for info on the technique and so far haven't found a thing. So.... What is going on when people laminate glass as in the work by James Shaw and Steve Ledterman? Is the glass fused together or are they gluing things together like some optical lenses?
Thanks and hiyas!
Karl
Posted: Mon Sep 22, 2003 10:04 pm
by Ron Coleman
Re: Laminated Glass?
Posted: Tue Sep 23, 2003 8:40 am
by Bert Weiss
K Boggs wrote:I have been hunting around for info on the technique and so far haven't found a thing. So.... What is going on when people laminate glass as in the work by James Shaw and Steve Ledterman? Is the glass fused together or are they gluing things together like some optical lenses?
Thanks and hiyas!
Karl
Hxtal epoxy. $1000 per gallon at HIS glassworks. That was the price, last I knew, a few years ago.