Page 1 of 1
devit spray maturation temps
Posted: Fri Sep 26, 2003 10:54 pm
by Liam
I am curently using borax as devit spray. It seems to me that there was a thread about a year ago about borax not maturing untill fairly hot temperatures were used. So does anyone know the minumum temperature for using borax, and, if I need to go cooler for just slumping, what spray should I use?
Thanks
Liam
Re: devit spray maturation temps
Posted: Sat Sep 27, 2003 8:06 pm
by Bert Weiss
Liam wrote:I am curently using borax as devit spray. It seems to me that there was a thread about a year ago about borax not maturing untill fairly hot temperatures were used. So does anyone know the minumum temperature for using borax, and, if I need to go cooler for just slumping, what spray should I use?
Thanks
Liam
Liam
It works for me at 1400ºF. I have not tried to push it lower so I can't comment.