Has anyone used the braided fiber robe? What is it good for. A dam to keep round pieces shape and thickness??
Thanks Lisa W
[/img]

Posted: Wed Oct 01, 2003 3:01 pm
by Brock
It's usually used as a gasket to prevent heat loss, around kiln lids, for instance. As a robe, it's too scratchy! Brock