Page 1 of 1

BE 1401 Clear

Posted: Mon Oct 06, 2003 6:56 am
by tom suter
I just fired a small tile with this crystal clear. I was really suprised when it came out with a ugly yellow tint to it. Anyone clue me in why this is?
Thanks for any help

Posted: Mon Oct 06, 2003 7:05 am
by Tom White
Sounds like silver stain. Have you ever fired anything with silver on your kiln shelf?

Best wishes,
Tom in Texas

Posted: Mon Oct 06, 2003 4:52 pm
by tom suter
never have fired anything with silver in the kiln. I just pulled the piece of glass that I got directly from be connection. I just called them up and it was a missed label glass. It had 1401 in a black marker but the sticker had 1320. My cataloque did not show 1320 but it was a marigold color. Thank God because I got about 2 full sheets of this. I think the piece I actuall pulled came out of their fusing crate you can buy and was just label wrong. I was really displease with my results of 0122 chips fired on this. I am not a yellow fan. Thanks