Designs on dichroic glass

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Robert Cohen

Designs on dichroic glass

Post by Robert Cohen »

I was following a thread about designs on dichro when I came across a response talking about using etching cream. What is etching cream? How do you use it? Where can you get it?

Any and all help will be appreciated! Thanks,

Bob :?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

Etchall: http://www.etchall.com/store/etching_creme.htm

Armour Etch: http://www.armourproducts.com/

Both are products you spread on the glass for a while, then clean off.
Tim Swann
Posts: 83
Joined: Mon Mar 10, 2003 9:47 pm
Location: San Diego, CA

Post by Tim Swann »

Bob,

You can get etching cream at Michaels in Arizona. They sell Armour in different size containers.

Tim