Confetti
Posted: Sat Oct 18, 2003 11:32 am
Can anybody tell me if I can use 90 coe confetti with 96 in a tack fuse, also is 96 confetti available? I would like to know before I go out and buy some.
Val
Val
Guide to fusing, slumping, and related kilnforming techniques
https://warmglass.com/phpBB3/
Possibly. The worst that will happen, is that the confetti may flake off the substrate. There will not be enough voliume of confetti to break the piece.Val wrote:Can anybody tell me if I can use 90 coe confetti with 96 in a tack fuse, also is 96 confetti available? I would like to know before I go out and buy some.
Val