Ferro troubleshooting guide

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Ferro troubleshooting guide

Post by Don Burt »

I saw this page on Ferro's site. I don't remember ever seeing it referenced here.
If your enamel work suffers from chain marks, crizzle, fish eyes, hickeys or whiskering, check it out

Ferro Troublehsooting Guide
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Post by rosanna gusler »

hickey: A, hormones.........B, adolescence...........C, 8 pack of schaenling (sp) little king cream ales
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Post by Don Burt »

rosanna gusler wrote:hickey: A, hormones.........B, adolescence...........C, 8 pack of schaenling (sp) little king cream ales
Schoenling. BUt I drank Strohs in the hickey years. Worse than cadmium/lead poisoning from Reusche enamels. (or actually might be identical)
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Ferro troubleshooting guide

Post by Bert Weiss »

db wrote:I saw this page on Ferro's site. I don't remember ever seeing it referenced here.
If your enamel work suffers from chain marks, crizzle, fish eyes, hickeys or whiskering, check it out

Ferro Troublehsooting Guide
I haven't checked it out yet, but they sound like effects we Ahtists are trying to get.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions