Page 1 of 1

Devit only with certain colors

Posted: Fri Oct 24, 2003 9:55 am
by maggie may
Hi,
I've been reading about devit in the archives and don't really know what to do with my problem. I'm using Bullseye Glass and don't have any devit problems with any colors except the orange and the coral colors. I also don't have it on every piece. Am I maybe leaving some film of dish washing detergent when I wash the pieces before fusing? After washing I wash them again with acetone. I have't used the Borax solution yet and don't really want to if I don't have to. Does anyone have any suggestions? Thanks
Marilyn

Posted: Fri Oct 24, 2003 11:46 am
by Geri Comstock
SuperSpray is the answer.

There's lots in the archives about various methods of application.

Geri