Page 1 of 1

Re: compatibility

Posted: Mon Dec 17, 2007 11:25 am
by rosanna gusler
sure. you can fuse any glasses together. why? rosanna

Re: compatibility

Posted: Mon Dec 17, 2007 1:04 pm
by Barry Kaiser
Question was asked on another furum and everyone answered no.

I just thought it might be possible.....small pieces....small stress nodes.