uh....duh! Me soo dumb sometime.Valerie Adams wrote:I made some single layer dish sets this year out of textured Spectrum non-fusible. I firepolished the edges first and then slumped. They're nice and smooth but still retain all their texture. I put the texture down on the shelf so the smooth side was the top.AndyT wrote:I have a ton of offcut textures as well and the main problem I've been having when trying to slump is that the edges don't come out smooth enough for my liking. The textures pretty much go away at higher temps...can't figure out the right temp to be to keep the texture and still have nice polished edges.