Post by The Hobbyist »

Switch from 1/8" fp to 1/16" fp and it will work well.

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: kilncarving

Post by rosanna gusler »

Linda Steider wrote:I teach kilncarving in my basic class & let the students go 3 to 5 layers high with fiber paper, using 2 layers of 3mm. We don't prefire to fuse first, just design, cut & stack the fp, place glass atop & fire. As Rosanna said, the firing schedule would be helpful, but without it I'd guess firing too fast; &/or could there have been too much glue under that high point that may have caused excess air?

Linda
the glue has outgassed well before the glass moves . rosanna