Post by gb »

Is 20 Mule Team BORAX natural laundry booster what is used to make devit solution? If not where do I get plain BORAX?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

There are two types of the 20 Mule Team. One is pure borax, the other has additives. Check and see if you have the one that's 100% borax.

If you don't and can't find it, most pottery supply places will have borax.