Page 1 of 1

Melting wine/beer bottles

Posted: Tue Nov 18, 2003 5:20 pm
by LynArts
I want to melt wine/beer bottle in my kiln. Does anyone out there know what cone (temperature) I need to shoot for? I hate the thought of having to watch them every minute. My kiln has a kiln-sitter, but not the new computer one. I did this in a former life but can't remember what temp. was good. Thanks for any help. lyn

Posted: Tue Nov 18, 2003 5:29 pm
by charlie
1525 for 10 minutes

Posted: Tue Nov 18, 2003 5:33 pm
by Brad Walker
Click on Search at the top of the page. Enter bottle into the form. You'll get more information about this subject than you probably wanted.