help for float
Moderators: Brad Walker, Tony Smith
help for float
i was given a 1/4 inch round float blank that is topped with float cullet and frit - size of blank is approx 12 "........need to first fuse it then slump over a ss bowl.......im under the weather with this flu and no patience to sit and search archives.....can anyone help me out here so i can get this fired up for someone.... 
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Doc
Lots of variables. What look do you want? How rounded do you want the edges. Is the tin side down (it should be). I would fire to 1420 with a 20 - 40 minute soak. Lower temp with longer soak yields a similar look to a higher temp and short soak, but the bottom comes out cleaner. I would ramp up to 1000 in about an hour or hour and a half, soak at 1240 for maybe 20 or 30 minutes and go to top. You don't say what thickness I would probably soak at 1000 for a half an hour to an hour, take that same time down to 900 than 3/4 of the time down to 700 and that same time down to 300.
Get well. Fire when you are thinking clearly.
Lots of variables. What look do you want? How rounded do you want the edges. Is the tin side down (it should be). I would fire to 1420 with a 20 - 40 minute soak. Lower temp with longer soak yields a similar look to a higher temp and short soak, but the bottom comes out cleaner. I would ramp up to 1000 in about an hour or hour and a half, soak at 1240 for maybe 20 or 30 minutes and go to top. You don't say what thickness I would probably soak at 1000 for a half an hour to an hour, take that same time down to 900 than 3/4 of the time down to 700 and that same time down to 300.
Get well. Fire when you are thinking clearly.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact: