I have a Skutt HotStart Kiln. Does anyone know how to add annealing time or change the ramping schedule at the beginning of the program?

Many thanks in advance. . .

Mira

Posted: Tue Dec 16, 2003 6:24 am
by All Fired Up
It can't be done on the 96. I have a 96 and I wanted to do the same. I called Skutt ane Perry told me that the only thing that can be changed is the high temp and holding time. The only other thing you can change is skipping a segment.