Page 1 of 1

frits and graniglia

Posted: Tue Dec 16, 2003 6:14 am
by mikefromitaly
hello friends,what is difference between frits and "graniglia"?

bue

Posted: Tue Dec 16, 2003 8:58 am
by judith
Hi,

I am not familiar with the term "graniglia"..........perhhaps it is Italian for small pieces of glass (frit)?

judith

Re: frits and graniglia

Posted: Tue Dec 16, 2003 11:34 am
by Brad Walker
mike77 wrote:hello friends,what is difference between frits and "graniglia"?
Frit is English, Graniglia is Italian.

Both mean small pieces of glass. Most often, "graniglia" refers to small pieces of glass that have been fused or melted together but still leaving a rough or granular texture on the outside. Kind of like tack fusing frit onto a sheet of glass, but not necessarily made that way.

Posted: Tue Dec 16, 2003 11:44 am
by Ed Burck