Posted: Sat Dec 20, 2003 7:17 pm
by Brad Walker
Has anyone tried thinfire on top of the Skamol board? How did it work?
Posted: Sat Dec 20, 2003 11:10 pm
by Marty
Brad- I don't use thinfire, just 972 paper, and I don't see where there would be any adverse affects from using tf on Skamol board. Sand the pressed verm. as fine as you need and fire-n-go (tm). Use the same precautions as you would on fiberboard. Marty
Posted: Sat Dec 20, 2003 11:34 pm
by Brad Walker
Yeah, that's what I think, too. I don't use thinfire either, but someone asked about if it would work with the Skamol board. I don't see any reason why it wouldn't, just thought I'd see if anyone had actually tried it.