I have been reading the "At My Wits End" series of emails and as someone fairly new to the world of warm glass, I have a very basic (and perhaps stupid) question.
What exactly is a pot melt?

Thanks for your help.

Posted: Thu Dec 25, 2003 2:39 pm
by Brock
Hey Bob, stack a bunch of cut pieces of glass in a garden variety ceramic (terra-cotta) pot, (widen/shape the drain hole) elevated over a shelf. The glass melts and pours out in a stream, slowly forming a pancake. Brock

Re: Pot Melts

Posted: Fri Dec 26, 2003 11:53 am
by jim simmons
Robert Cohen wrote:I have been reading the "At My Wits End" series of emails and as someone fairly new to the world of warm glass, I have a very basic (and perhaps stupid) question.
What exactly is a pot melt?

Thanks for your help.
Go to the archives and do a search on pot melt.
You will get a lot of info. \:D/
Jim

Pot Melts

Posted: Fri Dec 26, 2003 4:14 pm
by Robert Cohen
Thanks for the advice. Now I know what to do with all the broken glass I've been collecting.