Page 1 of 1

fiberglass

Posted: Tue Dec 30, 2003 2:54 pm
by slats
Is it possible to use fiberglass for making molds for slumping?

Posted: Wed Dec 31, 2003 12:46 pm
by Tony Serviente
To stiffen fiberglass you have to use a resin/hardner that would burn out well below slump temps. Even if you somehow rigidized it, your form would be moving as well as glass you wanted to slump.

Posted: Wed Dec 31, 2003 11:45 pm
by Tom White
The only practical use of fiberglass for a slumping mold I have heard of is the use of borosilicate glass fibers in a plaster/silica mold to strengthen it and prevent cracking while firing. BTW, contacte me directly again, the email I sent to you bounced.

Best wishes,
Tom in Texas