Anyone use "527 Cement" to Glue on Bails to Fused
Has anyone used this product?  I was told by my stained glass store that it is very good for fusing bails to glass (fused).  I've been using E6000 and it sometimes comes off with humidity and perspiration.  Any one have 527 experience?
			
			
									
						
										
						I use 527 for for adhering glass onto glass for layering effects. The glass has popped off occasionally even with 527 when I use some force (xacto knife to clean up oozed out glue) or when cleaning with wet sponge after I have grouted a mosaic for example.
I have had better luck with 527 overall percentage-wise than E6000.
Hope this helps.
Robin
			
			
									
						
										
						I have had better luck with 527 overall percentage-wise than E6000.
Hope this helps.
Robin
- 
				Alecia Helton
 - Posts: 108
 - Joined: Mon Aug 25, 2003 12:35 am
 - Location: outside of Dallas TX
 
- 
				Susan Moore
 - Posts: 96
 - Joined: Mon Oct 06, 2003 10:07 pm
 - Location: Austin, TX
 - Contact:
 
Dolores,
What brand of 5 minute epoxy are you using?
I have tried a 5 minute epoxy to glue sterling bails onto glass pendants and I could easily pull the bails off the pendants (20 or so) after the prescribed 16-hour waiting time. I am wondering if it was the brand I used or more likely an example of user error - I thought I mixed it very well but maybe my idea of thoroughly mixing is not sufficient. The epoxy stuck to the glass but not a bit of it stuck to the sterling bail that was scuffed and cleaned with rubbing alcohol. I switched back to E-6000 and it gives a very good hold for this particular application. I do prefer the ease of application of the epoxy though.
Susan
			
			
									
						
										
						What brand of 5 minute epoxy are you using?
I have tried a 5 minute epoxy to glue sterling bails onto glass pendants and I could easily pull the bails off the pendants (20 or so) after the prescribed 16-hour waiting time. I am wondering if it was the brand I used or more likely an example of user error - I thought I mixed it very well but maybe my idea of thoroughly mixing is not sufficient. The epoxy stuck to the glass but not a bit of it stuck to the sterling bail that was scuffed and cleaned with rubbing alcohol. I switched back to E-6000 and it gives a very good hold for this particular application. I do prefer the ease of application of the epoxy though.
Susan
- 
				Judy Schnabel
 - Posts: 195
 - Joined: Mon Mar 10, 2003 9:45 pm
 - Location: SW FL
 - Contact:
 
- 
				Susan Moore
 - Posts: 96
 - Joined: Mon Oct 06, 2003 10:07 pm
 - Location: Austin, TX
 - Contact:
 
Judy and Rodney thx for the info.  I will probably give epoxy another try.  I think when I use up my current supply of bails I would like to try and get off the adhesives altogether and use other means of attachment - wire wrapping, drilling holes, etc.  I envision less hassle and a more distinct look to my jewelry.
Susan
			
			
									
						
										
						Susan
- 
				Kevin Midgley
 - Posts: 773
 - Joined: Mon Mar 10, 2003 11:36 am
 - Location: Tofino, British Columbia, Canada
 
- 
				Judith Andre
 - Posts: 28
 - Joined: Thu Mar 20, 2003 2:38 am
 - Location: Lincoln, NE
 
- 
				Val Eibner
 - Posts: 19
 - Joined: Thu Jan 08, 2004 2:01 pm
 - Location: BC, Canada
 - Contact:
 
New to the forum and must say it is terrific for new comers to the art of hot glass.  Artist for 30 some years in clay and mix-media, but now have been bitten by the glass bug.  I am involved with a commissiom work that entails gluing on relief fused glass to a glass backing and I used what my glass supplier suggested which was a laminated gl on gl glue.  useless since 3 weeks after installing the piece on the wall a few of the smaller fused pieces fell on the floor breaking in front of the buyers eyes...not good for confidence so I am re-doing the whole piece.  Now what is the best adhesive to use outside of UV glue ..too pricey for now.  Read lots of debate over what one adhesive is the most reliable.   Sorry for the winded reply. Val
			
			
									
						
							Val
eibnerstudio
BC,Canada
			
						eibnerstudio
BC,Canada
I like plain old Silicone. Non-toxic, cheap, long lasting, available everywhere, holds a lot of weight, easy to use, etc,. etc, BrockVal Eibner wrote:New to the forum and must say it is terrific for new comers to the art of hot glass. Artist for 30 some years in clay and mix-media, but now have been bitten by the glass bug. I am involved with a commissiom work that entails gluing on relief fused glass to a glass backing and I used what my glass supplier suggested which was a laminated gl on gl glue. useless since 3 weeks after installing the piece on the wall a few of the smaller fused pieces fell on the floor breaking in front of the buyers eyes...not good for confidence so I am re-doing the whole piece. Now what is the best adhesive to use outside of UV glue ..too pricey for now. Read lots of debate over what one adhesive is the most reliable. Sorry for the winded reply. Val
- 
				rosanna gusler
 - Posts: 730
 - Joined: Mon Mar 10, 2003 2:22 pm
 - Location: wanchese north carolina
 - Contact: