Page 1 of 1

Skutt kiln lids problem with dropping pins

Posted: Fri Jan 16, 2004 3:51 pm
by Val Eibner
Followed up on some kiln information threads re: Pros and cons on kiln makes; and there was an annoying problem with the Skutt 1414 lid with pins dropping out during firing. Is this still a problem, because that is one of the kilns that I am looking at to buy. I have an oval ceramic kiln from Seattle Potter S. that I have used for 14 years with little or no problems then the normal wear. Do they make a good kiln? Does anyone out there have one to share with me their pros and cons on the crucible kiln. Thanks, Val :lol:

Posted: Fri Jan 16, 2004 5:05 pm
by Brad Walker
I have the 1414 and have never had the problem you mention.