Page 1 of 1
					
				Has anyone used new Spectrum S96 "high fire" irids
				Posted: Sat Jan 17, 2004 3:18 pm
				by Cliff Swanson
				Just seeking opinions, comparisons, rants, etc as to the URO coe 96 irids.
Thanks,
Cliff
			 
			
					
				
				Posted: Sat Jan 17, 2004 8:22 pm
				by RobinE
				Hi Cliff:
I am using the new Spectrum 96 Hi Fire Irids for a limited edition series of mine. So far colors available are black and clear. I understand white hi fire irid will be available soon.
The black hi fire looks good capped with clear or not. I prefer the look of the clear hi fire, irid side down onto another color.  They fire beautifully.
RobinE
			 
			
					
				
				Posted: Sun Jan 18, 2004 11:14 am
				by deb.co
				http://community.webshots.com/photo/112 ... 5523GMYbWG
I've been using the black Hi-Fire and I'm very happy with it!  On the picture you can see what it looks like capped and not capped.  I've got the clear also, but I have not experimented with it yet.