Page 1 of 1
					
				Schedule: is it to slow?
				Posted: Sun Jan 18, 2004 2:07 pm
				by Sean Albert
				I wrote in a few weeks ago about having trouble with BE devitrifying in an older kiln. I brought the kiln up to a high temp to “cleanâ€
			 
			
					
				Re: Schedule: is it to slow?
				Posted: Sun Jan 18, 2004 2:27 pm
				by Catharine Newell
				[quote="Sean Albert"]I wrote in a few weeks ago about having trouble with BE devitrifying in an older kiln. I brought the kiln up to a high temp to “cleanâ€
			 
			
					
				
				Posted: Sun Jan 18, 2004 2:57 pm
				by Catharine Newell
				And....  ramp up AFAP from 1240 (or whatever works for you) to your full fuse - again, taking the work quickly thru the 1300 devit range.  Don't dilly dally there!
Catharine
			 
			
					
				
				Posted: Sun Jan 18, 2004 8:55 pm
				by Sean Albert
				Thanks so much Catharine, I'll give it a try and let you know how it turns out. Sean.