What is the best way to attach/hold elements in the top of a frax kiln? And where could I buy them?

Thanks in advance.
BobB
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: attaching elements in a frax kiln

Post by Brad Walker »

BobB wrote:What is the best way to attach/hold elements in the top of a frax kiln? And where could I buy them?
One option is quartz tubes, available at http://www.duralite.com, http://www.quartz.com

Another option is mullite rods and "donuts", available at http://www.joppaglass.com

For wire use nichrome or stainless steel welding wire.