Page 1 of 1
Recalibrate Temp Controller?
Posted: Wed Jan 21, 2004 3:32 pm
by Judi R
Hello gang of glass -
My small kiln's temperature controller somehow got all whacked out and no longer gives me an accurate temp read.

Any ideas how to reset / readjust? Unfortunately, I've lost all the literature that came with it.
Thanks! - Judi
Re: Recalibrate Temp Controller?
Posted: Wed Jan 21, 2004 3:40 pm
by Brock
jjrentschler wrote:Hello gang of glass -
My small kiln's temperature controller somehow got all whacked out and no longer gives me an accurate temp read.

Any ideas how to reset / readjust? Unfortunately, I've lost all the literature that came with it.
Thanks! - Judi
If it's a pyrometer/thermocouple, there will be a screw on the pyrometer face. Put the thermocouple in boiling water and turn the screw to read 212.
That should work okay, although there is room for error, the hotter you go. If it's a controller, get it done by the manufacturer. Brock